Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 14.4 % Show Material materials with Dehnung of 14.4 % | Predicted Value, A200 | ||||
19.9 % Show Material materials with Dehnung of 19.9 % | Predicted Value, A5 | |||||
21.7 % Show Material materials with Dehnung of 21.7 % | Predicted Value, A50 | |||||
21.7 % Show Material materials with Dehnung of 21.7 % | Predicted Value, Transverse | |||||
22.4 % Show Material materials with Dehnung of 22.4 % | Predicted Value | |||||
20 °C | 33 % Show Material materials with Dehnung of 33 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 35 % Show Material materials with Dehnung of 35 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 37 % Show Material materials with Dehnung of 37 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 37 % Show Material materials with Dehnung of 37 % | skin passed | EN 10152 | Strip, Sheet | A80 | |
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Flächenreduzierung | 42.0 % Show Material materials with Flächenreduzierung of 42.0 % | Predicted Value | ||||
43.5 % Show Material materials with Flächenreduzierung of 43.5 % | Predicted Value, Transverse | |||||
Härte, Brinell | 266 [-] Show Material materials with Härte, Brinell of 266 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||||
Scherfestigkeit | 562.8 MPa Show Material materials with Scherfestigkeit of 562.8 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 279.1 MPa Show Material materials with Streckgrenze of 279.1 MPa | Predicted Value, RP05 | ||||
286.5 MPa Show Material materials with Streckgrenze of 286.5 MPa | Predicted Value, RP1 Transverse | |||||
293.2 MPa Show Material materials with Streckgrenze of 293.2 MPa | Predicted Value, RP1 | |||||
364.4 MPa Show Material materials with Streckgrenze of 364.4 MPa | Predicted Value, RP02 Transverse | |||||
546.1 MPa Show Material materials with Streckgrenze of 546.1 MPa | Predicted Value, RP02 | |||||
627.3 MPa Show Material materials with Streckgrenze of 627.3 MPa | Predicted Value, RP002 | |||||
20 °C | 140 - 260 MPa Show Material materials with Streckgrenze of 140 - 260 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 240 MPa Show Material materials with Streckgrenze of 140 - 240 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 220 MPa Show Material materials with Streckgrenze of 140 - 220 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 220 MPa Show Material materials with Streckgrenze of 140 - 220 MPa | skin passed | EN 10152 | Strip, Sheet | ||
Zugfestigkeit | 20 °C | 270 - 350 MPa Show Material materials with Zugfestigkeit of 270 - 350 MPa | skin passed | EN 10152 | Strip | Transverse |
20 °C | 270 - 350 MPa Show Material materials with Zugfestigkeit of 270 - 350 MPa | skin passed | EN 10152 | Strip, Sheet |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 364.5 °C Show Material materials with Max. Betriebstemperatur of 364.5 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 8 S/m Show Material materials with Elektrische Leitfähigkeit of 8 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | skin passed | EN 10152 | Strip, Sheet |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % | skin passed | EN 10152 | Strip, Sheet |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | skin passed | EN 10152 | Strip, Sheet |