Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A80 | 20.0 °C | 34 % Show Material materials with Dehnung A80 of 34 % | |
Dehnung A80, transversal | 20.0 °C | 30 - 34 % Show Material materials with Dehnung A80, transversal of 30 - 34 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Streckgrenze | 20.0 °C | 140 - 240 MPa Show Material materials with Streckgrenze of 140 - 240 MPa | |
Streckgrenze, transversal | 20.0 °C | 140 - 280 MPa Show Material materials with Streckgrenze, transversal of 140 - 280 MPa | |
Zugfestigkeit | 20.0 °C | 270 - 370 MPa Show Material materials with Zugfestigkeit of 270 - 370 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 270 - 370 MPa Show Material materials with Zugfestigkeit, transversal of 270 - 370 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties