Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 7 % Show Material materials with Dehnung of 7 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 20.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 1550 MPa Show Material materials with Streckgrenze Rp 0,2 of 1550 MPa | |
Zugfestigkeit | 20.0 °C | 1600 - 1900 MPa Show Material materials with Zugfestigkeit of 1600 - 1900 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 - 0.8 % Show Material materials with Chrom of 0.4 - 0.8 % |
Kohlenstoff | 0.4 - 0.5 % Show Material materials with Kohlenstoff of 0.4 - 0.5 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 1.3 - 1.7 % Show Material materials with Silizium of 1.3 - 1.7 % |
Vanadium | 0.1 - 0.25 % Show Material materials with Vanadium of 0.1 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |