Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 25 % Show Material materials with Dehnung of 25 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Härte, Brinell | 20.0 °C | 311 [-] Show Material materials with Härte, Brinell of 311 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 500 MPa Show Material materials with Streckgrenze Rp 0,2 of 500 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 540 MPa Show Material materials with Streckgrenze Rp 1,0 of 540 MPa | |
Zugfestigkeit | 20.0 °C | 850 - 1050 MPa Show Material materials with Zugfestigkeit of 850 - 1050 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | |
400.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ||
600.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | ||
800.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | ||
1000.0 °C | 1.95E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.95E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 1150 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 1150 °C | ||
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 14.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14.5 W/(m·K) | |
500.0 °C | 20 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 20 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 7.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 7.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.2 - 0.3 % Show Material materials with Kohlenstoff of 0.2 - 0.3 % |
Mangan | 8 - 10 % Show Material materials with Mangan of 8 - 10 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.2 - 0.4 % Show Material materials with Stickstoff of 0.2 - 0.4 % |