Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8 g/cm³ Show Material materials with Dichte of 8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | Typical for Duplex Stainless Steel |
Härte, Brinell | 20.0 °C | 200 [-] Show Material materials with Härte, Brinell of 200 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 270 MPa Show Material materials with Streckgrenze Rp 0,2 of 270 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 300 MPa Show Material materials with Streckgrenze Rp 1,0 of 300 MPa | |
Zugfestigkeit | 20.0 °C | 500 - 650 MPa Show Material materials with Zugfestigkeit of 500 - 650 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.55E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.55E-5 1/K | |
400.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | ||
600.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | ||
800.0 °C | 1.77E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.77E-5 1/K | ||
1000.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ||
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Max. Betriebstemperatur, lang | 0 - 1100 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 1100 °C | ||
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 12 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 W/(m·K) | |
500.0 °C | 19.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19.5 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1E-6 Ω·m Show Material materials with spezifischer Widerstand of 1E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 20 - 23 % Show Material materials with Chrom of 20 - 23 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Nickel | 33 - 37 % Show Material materials with Nickel of 33 - 37 % |
Niobium | 1 - 1.5 % Show Material materials with Niobium of 1 - 1.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 - 2 % Show Material materials with Silizium of 1 - 2 % |
Stickstoff | 0.11 % Show Material materials with Stickstoff of 0.11 % |