Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 15 % Show Material materials with Dehnung of 15 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 540 MPa Show Material materials with Streckgrenze Rp 0,2 of 540 MPa | |
100.0 °C | 515 MPa Show Material materials with Streckgrenze Rp 0,2 of 515 MPa | ||
200.0 °C | 485 MPa Show Material materials with Streckgrenze Rp 0,2 of 485 MPa | ||
300.0 °C | 455 MPa Show Material materials with Streckgrenze Rp 0,2 of 455 MPa | ||
Zugfestigkeit | 20.0 °C | 760 - 960 MPa Show Material materials with Zugfestigkeit of 760 - 960 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.08E-5 - 1.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.08E-5 - 1.1E-5 1/K | |
200.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | ||
300.0 °C | 1.15E-5 - 1.25E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.15E-5 - 1.25E-5 1/K | ||
400.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | ||
500.0 °C | 1.2E-5 - 1.35E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 - 1.35E-5 1/K | ||
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 50.0 °C | 17 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 17 W/(m·K) | |
100.0 °C | 18 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18 W/(m·K) | ||
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17 % Show Material materials with Chrom of 15 - 17 % |
Kohlenstoff | 0.06 % Show Material materials with Kohlenstoff of 0.06 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.7 - 1.5 % Show Material materials with Molybdän of 0.7 - 1.5 % |
Nickel | 4 - 6 % Show Material materials with Nickel of 4 - 6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |