Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 16 % Show Material materials with Dehnung of 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 420 MPa Show Material materials with Streckgrenze Rp 0,2 of 420 MPa | |
200.0 °C | 390 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 MPa | ||
300.0 °C | 380 MPa Show Material materials with Streckgrenze Rp 0,2 of 380 MPa | ||
400.0 °C | 370 MPa Show Material materials with Streckgrenze Rp 0,2 of 370 MPa | ||
500.0 °C | 305 MPa Show Material materials with Streckgrenze Rp 0,2 of 305 MPa | ||
550.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa | ||
Streckgrenze Rp 1,0 | 20.0 °C | 210 MPa Show Material materials with Streckgrenze Rp 1,0 of 210 MPa | |
Zugfestigkeit | 20.0 °C | 630 - 760 MPa Show Material materials with Zugfestigkeit of 630 - 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.18E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.18E-5 1/K | |
300.0 °C | 1.23E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.23E-5 1/K | ||
500.0 °C | 1.27E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.27E-5 1/K | ||
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 50.0 °C | 30.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30.1 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 4 - 6 % Show Material materials with Chrom of 4 - 6 % |
Kohlenstoff | 0.12 - 0.19 % Show Material materials with Kohlenstoff of 0.12 - 0.19 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |