EN 10213 Grade GX3CrNi13-4 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

Material GX3CrNi13-4 is equivalent to trademark G-X 3 CrNi 13 4 acc. to SEW 685-89. It combines high strength and very good cryogenic properties. It is used at low temperatures in refrigerator construction up to approx. -120 °C. Material G-X 5 CrNi 13 4, material number 1.4313 is acc. to VdTÜV-material specification 452 applicable for pressure vessels acc. to TRB 100 (and AD-data sheets W5 and W10) from -120 to 20 °C. Further application for blade and guide wheels for pumps, compressors and turbines as well as for pump casings and machine components in hydraulic installations from -120 to 20 °C. Further application in the nuclear power engineering if the relevant specifications allow the application at -120 to 20 °C. The welding suitability of the steel cast is examined for the welding methods TIG-welding, metal arc welding and submerged welding. After the welding the material have to cool down under 80 deg. for an following heat-treatment. An double tempering or stress relieve annealing is possible. After the double tempering an decrease of the strength should considered. The cooling rate until below 300 °C should not exceed 80 K/h. By the welding in the production of thin-walled parts its possible to abandon the pre-heating, tempering or stress relieve annealing if appropriate verification was done.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

7.7 g/cm³

Show Material materials with Dichte of 7.7 g/cm³

Mechanisch

PropertyTemperatureValueComment

Dehnung

20.0 °C

15 %

Show Material materials with Dehnung of 15 %

Elastizitätsmodul

23.0 °C

190 - 210 GPa

Show Material materials with Elastizitätsmodul of 190 - 210 GPa

Typical for Steel

Poissonzahl

23.0 °C

0.3 [-]

Show Material materials with Poissonzahl of 0.3 [-]

Typical for Steel

Streckgrenze Rp 0,2

20.0 °C

500 MPa

Show Material materials with Streckgrenze Rp 0,2 of 500 MPa

100.0 °C

515 MPa

Show Material materials with Streckgrenze Rp 0,2 of 515 MPa

150.0 °C

500 MPa

Show Material materials with Streckgrenze Rp 0,2 of 500 MPa

200.0 °C

485 MPa

Show Material materials with Streckgrenze Rp 0,2 of 485 MPa

250.0 °C

470 MPa

Show Material materials with Streckgrenze Rp 0,2 of 470 MPa

300.0 °C

455 MPa

Show Material materials with Streckgrenze Rp 0,2 of 455 MPa

Zugfestigkeit

20.0 °C

700 - 900 MPa

Show Material materials with Zugfestigkeit of 700 - 900 MPa

Thermisch

PropertyTemperatureValue

Koeffizient der thermischen Ausdehnung

-195.0 °C

8.6E-6 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 8.6E-6 1/K

-170.0 °C

9.3E-6 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 1/K

-120.0 °C

1.01E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.01E-5 1/K

-50.0 °C

1.08E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.08E-5 1/K

-25.0 °C

1.1E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 1/K

100.0 °C

1.05E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.05E-5 1/K

300.0 °C

1.1E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 1/K

500.0 °C

1.2E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K

Unlock all property charts

Max. Betriebstemperatur, lang

-120 - 20 °C

Show Material materials with Max. Betriebstemperatur, lang of -120 - 20 °C

Spezifische Wärmekapazität

20.0 °C

460 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K)

Wärmeleitfähigkeit

-20.0 °C

30 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 30 W/(m·K)

50.0 °C

26 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 26 W/(m·K)

100.0 °C

27 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 27 W/(m·K)

Unlock all property charts

Chemical properties

PropertyValue

Chrom

12 - 13.5 %

Show Material materials with Chrom of 12 - 13.5 %

Kohlenstoff

0.05 %

Show Material materials with Kohlenstoff of 0.05 %

Kupfer

0.3 %

Show Material materials with Kupfer of 0.3 %

Mangan

1 %

Show Material materials with Mangan of 1 %

Molybdän

0.7 %

Show Material materials with Molybdän of 0.7 %

Nickel

3.5 - 5 %

Show Material materials with Nickel of 3.5 - 5 %

Phosphor

0.04 %

Show Material materials with Phosphor of 0.04 %

Schwefel

0.015 %

Show Material materials with Schwefel of 0.015 %

Silizium

1 %

Show Material materials with Silizium of 1 %

Vanadium

0.08 %

Show Material materials with Vanadium of 0.08 %