Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 19 % Show Material materials with Dehnung of 19 % | |
Dehnung, transversal | 20.0 °C | 17 % Show Material materials with Dehnung, transversal of 17 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Molybdenum Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 400 MPa | |
100.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
150.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
200.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
250.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
300.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
350.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
400.0 °C | 368 MPa Show Material materials with Streckgrenze Rp 0,2 of 368 MPa | ||
Streckgrenze Rp 0,2, transversal | 20.0 °C | 400 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 400 MPa | |
Zugfestigkeit | 20.0 °C | 540 - 690 MPa Show Material materials with Zugfestigkeit of 540 - 690 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 540 - 690 MPa Show Material materials with Zugfestigkeit, transversal of 540 - 690 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.29E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.29E-5 1/K | Typical for Molybdenum Steel |
Max. Betriebstemperatur, lang | 200 - 550 °C Show Material materials with Max. Betriebstemperatur, lang of 200 - 550 °C | ||
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 37 - 48 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.06 % Show Material materials with Aluminium of 0.06 % |
Bor | 2E-3 - 6E-3 % Show Material materials with Bor of 2E-3 - 6E-3 % |
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % |
Kohlenstoff | 0.06 - 0.1 % Show Material materials with Kohlenstoff of 0.06 - 0.1 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.6 - 0.8 % Show Material materials with Mangan of 0.6 - 0.8 % |
Molybdän | 0.4 - 0.5 % Show Material materials with Molybdän of 0.4 - 0.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 - 0.02 % Show Material materials with Schwefel of 0.01 - 0.02 % |
Silizium | 0.1 - 0.35 % Show Material materials with Silizium of 0.1 - 0.35 % |
Titan | 0.06 % Show Material materials with Titan of 0.06 % |