Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 22 % Show Material materials with Dehnung of 22 % |
Dehnung, transversal | 20.0 °C | 20 % Show Material materials with Dehnung, transversal of 20 % |
Streckgrenze Rp 0,2 | 20.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 MPa |
100.0 °C | 156 MPa Show Material materials with Streckgrenze Rp 0,2 of 156 MPa | |
150.0 °C | 150 MPa Show Material materials with Streckgrenze Rp 0,2 of 150 MPa | |
200.0 °C | 148 MPa Show Material materials with Streckgrenze Rp 0,2 of 148 MPa | |
250.0 °C | 147 MPa Show Material materials with Streckgrenze Rp 0,2 of 147 MPa | |
300.0 °C | 145 MPa Show Material materials with Streckgrenze Rp 0,2 of 145 MPa | |
350.0 °C | 142 MPa Show Material materials with Streckgrenze Rp 0,2 of 142 MPa | |
400.0 °C | 137 MPa Show Material materials with Streckgrenze Rp 0,2 of 137 MPa | |
450.0 °C | 129 MPa Show Material materials with Streckgrenze Rp 0,2 of 129 MPa | |
500.0 °C | 116 MPa Show Material materials with Streckgrenze Rp 0,2 of 116 MPa | |
Streckgrenze Rp 0,2, transversal | 20.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 175 MPa |
Zugfestigkeit | 20.0 °C | 430 - 580 MPa Show Material materials with Zugfestigkeit of 430 - 580 MPa |
Zugfestigkeit, transversal | 20.0 °C | 430 - 580 MPa Show Material materials with Zugfestigkeit, transversal of 430 - 580 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur, lang | 0 - 550 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 550 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.04 % Show Material materials with Aluminium of 0.04 % |
Chrom | 4 - 6 % Show Material materials with Chrom of 4 - 6 % |
Kohlenstoff | 0.08 - 0.15 % Show Material materials with Kohlenstoff of 0.08 - 0.15 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 - 0.02 % Show Material materials with Schwefel of 0.01 - 0.02 % |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % |