Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 14 - 16 % Show Material materials with Dehnung of 14 - 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Streckgrenze | 20.0 °C | 420 MPa Show Material materials with Streckgrenze of 420 MPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 405 MPa Show Material materials with Streckgrenze Rp 0,2 of 405 MPa | |
100.0 °C | 345 MPa Show Material materials with Streckgrenze Rp 0,2 of 345 MPa | ||
150.0 °C | 335 MPa Show Material materials with Streckgrenze Rp 0,2 of 335 MPa | ||
200.0 °C | 327 MPa Show Material materials with Streckgrenze Rp 0,2 of 327 MPa | ||
250.0 °C | 323 MPa Show Material materials with Streckgrenze Rp 0,2 of 323 MPa | ||
300.0 °C | 322 MPa Show Material materials with Streckgrenze Rp 0,2 of 322 MPa | ||
350.0 °C | 316 MPa Show Material materials with Streckgrenze Rp 0,2 of 316 MPa | ||
400.0 °C | 306 MPa Show Material materials with Streckgrenze Rp 0,2 of 306 MPa | ||
450.0 °C | 285 MPa Show Material materials with Streckgrenze Rp 0,2 of 285 MPa | ||
500.0 °C | 256 MPa Show Material materials with Streckgrenze Rp 0,2 of 256 MPa | ||
Zugfestigkeit | 20.0 °C | 640 - 780 MPa Show Material materials with Zugfestigkeit of 640 - 780 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 4 - 6 % Show Material materials with Chrom of 4 - 6 % |
Kohlenstoff | 0.18 % Show Material materials with Kohlenstoff of 0.18 % |
Mangan | 0.3 - 0.8 % Show Material materials with Mangan of 0.3 - 0.8 % |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |