Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 14 % Show Material materials with Dehnung of 14 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 630 - 690 MPa Show Material materials with Streckgrenze of 630 - 690 MPa | |
Streckgrenze Rp 0,2 | 50.0 °C | 610 - 670 MPa Show Material materials with Streckgrenze Rp 0,2 of 610 - 670 MPa | |
100.0 °C | 585 - 645 MPa Show Material materials with Streckgrenze Rp 0,2 of 585 - 645 MPa | ||
150.0 °C | 555 - 615 MPa Show Material materials with Streckgrenze Rp 0,2 of 555 - 615 MPa | ||
200.0 °C | 535 - 595 MPa Show Material materials with Streckgrenze Rp 0,2 of 535 - 595 MPa | ||
250.0 °C | 515 - 575 MPa Show Material materials with Streckgrenze Rp 0,2 of 515 - 575 MPa | ||
300.0 °C | 510 - 570 MPa Show Material materials with Streckgrenze Rp 0,2 of 510 - 570 MPa | ||
Zugfestigkeit | 20.0 °C | 720 - 940 MPa Show Material materials with Zugfestigkeit of 720 - 940 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.018 % Show Material materials with Aluminium of 0.018 % |
Bor | 5E-3 % Show Material materials with Bor of 5E-3 % |
Chrom | 1.5 % Show Material materials with Chrom of 1.5 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % |
Molybdän | 0.7 % Show Material materials with Molybdän of 0.7 % |
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % |
Niobium | 0.05 - 0.06 % Show Material materials with Niobium of 0.05 - 0.06 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 - 0.015 % Show Material materials with Schwefel of 0.01 - 0.015 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Vanadium | 0.12 % Show Material materials with Vanadium of 0.12 % |
Zirkonium | 0.15 % Show Material materials with Zirkonium of 0.15 % |