Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 15 % Show Material materials with Dehnung of 15 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Flächenreduzierung | 20.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 660 MPa Show Material materials with Streckgrenze Rp 0,2 of 660 MPa | |
50.0 °C | 642 MPa Show Material materials with Streckgrenze Rp 0,2 of 642 MPa | ||
100.0 °C | 624 MPa Show Material materials with Streckgrenze Rp 0,2 of 624 MPa | ||
150.0 °C | 603 MPa Show Material materials with Streckgrenze Rp 0,2 of 603 MPa | ||
200.0 °C | 595 MPa Show Material materials with Streckgrenze Rp 0,2 of 595 MPa | ||
250.0 °C | 581 MPa Show Material materials with Streckgrenze Rp 0,2 of 581 MPa | ||
300.0 °C | 573 MPa Show Material materials with Streckgrenze Rp 0,2 of 573 MPa | ||
350.0 °C | 559 MPa Show Material materials with Streckgrenze Rp 0,2 of 559 MPa | ||
400.0 °C | 537 MPa Show Material materials with Streckgrenze Rp 0,2 of 537 MPa | ||
450.0 °C | 508 MPa Show Material materials with Streckgrenze Rp 0,2 of 508 MPa | ||
500.0 °C | 464 MPa Show Material materials with Streckgrenze Rp 0,2 of 464 MPa | ||
550.0 °C | 406 MPa Show Material materials with Streckgrenze Rp 0,2 of 406 MPa | ||
600.0 °C | 334 MPa Show Material materials with Streckgrenze Rp 0,2 of 334 MPa | ||
Zugfestigkeit | 20.0 °C | 820 - 1000 MPa Show Material materials with Zugfestigkeit of 820 - 1000 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.015 - 0.08 % Show Material materials with Aluminium of 0.015 - 0.08 % |
Arsen | 0.02 % Show Material materials with Arsen of 0.02 % |
Bor | 0.001 - 0.01 % Show Material materials with Bor of 0.001 - 0.01 % |
Chrom | 0.9 - 1.2 % Show Material materials with Chrom of 0.9 - 1.2 % |
Kohlenstoff | 0.17 - 0.23 % Show Material materials with Kohlenstoff of 0.17 - 0.23 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.35 - 0.75 % Show Material materials with Mangan of 0.35 - 0.75 % |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 - 0.02 % Show Material materials with Schwefel of 0.015 - 0.02 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 0.07 - 0.15 % Show Material materials with Titan of 0.07 - 0.15 % |
Vanadium | 0.6 - 0.8 % Show Material materials with Vanadium of 0.6 - 0.8 % |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % |