Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze Rp 0,2 | 50.0 °C | 730 MPa Show Material materials with Streckgrenze Rp 0,2 of 730 MPa | |
100.0 °C | 680 MPa Show Material materials with Streckgrenze Rp 0,2 of 680 MPa | ||
150.0 °C | 668 MPa Show Material materials with Streckgrenze Rp 0,2 of 668 MPa | ||
200.0 °C | 655 MPa Show Material materials with Streckgrenze Rp 0,2 of 655 MPa | ||
250.0 °C | 653 MPa Show Material materials with Streckgrenze Rp 0,2 of 653 MPa | ||
300.0 °C | 650 MPa Show Material materials with Streckgrenze Rp 0,2 of 650 MPa | ||
350.0 °C | 630 MPa Show Material materials with Streckgrenze Rp 0,2 of 630 MPa | ||
400.0 °C | 610 MPa Show Material materials with Streckgrenze Rp 0,2 of 610 MPa | ||
450.0 °C | 560 MPa Show Material materials with Streckgrenze Rp 0,2 of 560 MPa | ||
500.0 °C | 505 MPa Show Material materials with Streckgrenze Rp 0,2 of 505 MPa | ||
550.0 °C | 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 400 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 11 - 12.5 % Show Material materials with Chrom of 11 - 12.5 % |
Kohlenstoff | 0.08 - 0.15 % Show Material materials with Kohlenstoff of 0.08 - 0.15 % |
Mangan | 0.4 - 0.9 % Show Material materials with Mangan of 0.4 - 0.9 % |
Molybdän | 1.5 - 2 % Show Material materials with Molybdän of 1.5 - 2 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.02 - 0.04 % Show Material materials with Stickstoff of 0.02 - 0.04 % |
Vanadium | 0.25 - 0.4 % Show Material materials with Vanadium of 0.25 - 0.4 % |