Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.15 g/cm³ Show Material materials with Dichte of 7.15 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 5 % Show Material materials with Dehnung of 5 % | |
Elastizitätsmodul | 20.0 °C | 165 - 190 GPa Show Material materials with Elastizitätsmodul of 165 - 190 GPa | |
Härte, Brinell | 20.0 °C | 300 - 360 [-] Show Material materials with Härte, Brinell of 300 - 360 [-] | |
Poissonzahl | 23.0 °C | 0.26 - 0.31 [-] Show Material materials with Poissonzahl of 0.26 - 0.31 [-] | Typical for Ductile (Nodular) Cast Iron |
Schubmodule | 23.0 °C | 63 - 66 GPa Show Material materials with Schubmodule of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Streckgrenze Rp 0,2 | 20.0 °C | 700 MPa Show Material materials with Streckgrenze Rp 0,2 of 700 MPa | |
Zugfestigkeit | 20.0 °C | 1000 MPa Show Material materials with Zugfestigkeit of 1000 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 400.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | |
Schmelzpunkt | 1150 - 1200 °C Show Material materials with Schmelzpunkt of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron | |
Spezifische Wärmekapazität | 20.0 °C | 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) | |
400.0 °C | 507 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 507 J/(kg·K) | ||
Wärmeleitfähigkeit | 20.0 °C | 33 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 33 W/(m·K) | |
300.0 °C | 33 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 33 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 5.4E-7 Ω·m Show Material materials with spezifischer Widerstand of 5.4E-7 Ω·m |