Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 19 - 26 % Show Material materials with Dehnung A5 of 19 - 26 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Schlagfestigkeit, Charpy gekerbt | -5.0 °C | 47 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 47 kJ/m² | |
Streckgrenze | 23.0 °C | 420 - 460 MPa Show Material materials with Streckgrenze of 420 - 460 MPa | |
Zugfestigkeit | 23.0 °C | 570 - 720 MPa Show Material materials with Zugfestigkeit of 570 - 720 MPa |