Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 20.0 °C | 17 % Show Material materials with Dehnung A5 of 17 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Schlagfestigkeit, Charpy gekerbt | -50.0 °C | 27 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 27 kJ/m² | |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 380 - 460 MPa Show Material materials with Streckgrenze Rp 0,2 of 380 - 460 MPa | |
Zugfestigkeit | 20.0 °C | 510 - 720 MPa Show Material materials with Zugfestigkeit of 510 - 720 MPa | |
impactTransVNotch | -50.0 °C | 16 kJ/m² Show Material materials with impactTransVNotch of 16 kJ/m² |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Curie-Temperatur | 20.0 °C | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.02 % Show Material materials with Aluminium of 0 - 0.02 % |
Bor | 0 - 5E-3 % Show Material materials with Bor of 0 - 5E-3 % |
Chrom | 0.7 - 2 % Show Material materials with Chrom of 0.7 - 2 % |
Eisen | 90.45 - 99.3 % Show Material materials with Eisen of 90.45 - 99.3 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.7 - 1.5 % Show Material materials with Kupfer of 0.7 - 1.5 % |
Mangan | 0.7 - 1.7 % Show Material materials with Mangan of 0.7 - 1.7 % |
Molybdän | 0.4 - 1 % Show Material materials with Molybdän of 0.4 - 1 % |
Nickel | 1 - 2 % Show Material materials with Nickel of 1 - 2 % |
Niobium | 0 - 0.06 % Show Material materials with Niobium of 0 - 0.06 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 - 0.03 % Show Material materials with Schwefel of 0.025 - 0.03 % |
Silizium | 0.5 - 0.55 % Show Material materials with Silizium of 0.5 - 0.55 % |
Stickstoff | 0 - 0.02 % Show Material materials with Stickstoff of 0 - 0.02 % |
Titan | 0 - 0.2 % Show Material materials with Titan of 0 - 0.2 % |
Vanadium | 0 - 0.2 % Show Material materials with Vanadium of 0 - 0.2 % |
Zirkonium | 0 - 0.15 % Show Material materials with Zirkonium of 0 - 0.15 % |
Technological properties
Property | ||
---|---|---|
Processing history | normalized, controlled rolled |