Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 16 % Show Material materials with Dehnung A5 of 16 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Schlagfestigkeit, Charpy gekerbt | -50.0 °C | 27 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 27 kJ/m² | |
-20.0 °C | 39 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 39 kJ/m² | ||
Streckgrenze Rp 0,2 | 23.0 °C | 530 - 550 MPa Show Material materials with Streckgrenze Rp 0,2 of 530 - 550 MPa | |
Zugfestigkeit | 23.0 °C | 650 - 830 MPa Show Material materials with Zugfestigkeit of 650 - 830 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | quenched and tempered |