Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.72 - 8 g/cm³ Show Material materials with Dichte of 7.72 - 8 g/cm³ | Typical for Tool And Machining Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 203 - 211 GPa Show Material materials with Elastizitätsmodul of 203 - 211 GPa | Typical for Tool And Machining Steel |
Härte, Vickers | 23.0 °C | 250 [-] Show Material materials with Härte, Vickers of 250 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Tool And Machining Steel |
Schubmodule | 23.0 °C | 79 GPa Show Material materials with Schubmodule of 79 GPa | Typical for Tool And Machining Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.3E-5 1/K | Typical for Tool And Machining Steel |
Schmelzpunkt | 1370 - 1425 °C Show Material materials with Schmelzpunkt of 1370 - 1425 °C | Typical for Tool And Machining Steel | |
Spezifische Wärmekapazität | 23.0 °C | 420 - 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 - 460 J/(kg·K) | Typical for Tool And Machining Steel |
Wärmeleitfähigkeit | 23.0 °C | 17 - 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 17 - 42 W/(m·K) | Typical for Tool And Machining Steel |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |