Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 23 % Show Material materials with Dehnung A5 of 23 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Schlagfestigkeit, Charpy gekerbt | 20.0 °C | 39 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 39 kJ/m² | |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa | |
Zugfestigkeit | 23.0 °C | 540 MPa Show Material materials with Zugfestigkeit of 540 MPa |