Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 30 % Show Material materials with Dehnung A5 of 30 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 195 MPa Show Material materials with Streckgrenze of 195 MPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 195 MPa Show Material materials with Streckgrenze Rp 0,2 of 195 MPa | |
Streckgrenze Rp 1,0 | 23.0 °C | 235 MPa Show Material materials with Streckgrenze Rp 1,0 of 235 MPa | |
Zugfestigkeit | 23.0 °C | 490 - 690 MPa Show Material materials with Zugfestigkeit of 490 - 690 MPa |