Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Abmessung
Property | Value |
---|---|
Wall thickness | 1 - 8 mm Show Material materials with Wall thickness of 1 - 8 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 21 - 30 % Show Material materials with Dehnung A5 of 21 - 30 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Molybdenum Steel |
Härte, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Härte, Rockwell B of 80 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Molybdenum Steel |
Streckgrenze | 23.0 °C | 205 MPa Show Material materials with Streckgrenze of 205 MPa | |
Zugfestigkeit | 23.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.29E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.29E-5 1/K | Typical for Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 37 - 48 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |