Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Abmessung
Property | Value |
---|---|
Wall thickness | 1 - 8 mm Show Material materials with Wall thickness of 1 - 8 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 14 - 30 % Show Material materials with Dehnung A5 of 14 - 30 % | |
Dehnung A5, transversal | 23.0 °C | 25 % Show Material materials with Dehnung A5, transversal of 25 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Zugfestigkeit | 23.0 °C | 290 MPa Show Material materials with Zugfestigkeit of 290 MPa |