Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 30 % Show Material materials with Dehnung A5 of 30 % |
Streckgrenze Rp 0,2 | 20.0 °C | 205 - 245 MPa Show Material materials with Streckgrenze Rp 0,2 of 205 - 245 MPa |
Zugfestigkeit | 20.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 17 % Show Material materials with Chrom of 14 - 17 % |
Eisen | 6 - 10 % Show Material materials with Eisen of 6 - 10 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 72 % Show Material materials with Nickel of 72 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-finished, annealed |