Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 35 % Show Material materials with Dehnung A5 of 35 % |
Streckgrenze Rp 0,2 | 20.0 °C | 175 - 205 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 - 205 MPa |
Zugfestigkeit | 20.0 °C | 520 - 590 MPa Show Material materials with Zugfestigkeit of 520 - 590 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 27 - 31 % Show Material materials with Chrom of 27 - 31 % |
Eisen | 7 - 11 % Show Material materials with Eisen of 7 - 11 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 58 % Show Material materials with Nickel of 58 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | hot-finished, annealed |