Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 0.15 - 0.6 % Show Material materials with Aluminium of 0.15 - 0.6 % |
Chrom | 19 - 23 % Show Material materials with Chrom of 19 - 23 % |
Eisen | 37.4 - 50.7 % Show Material materials with Eisen of 37.4 - 50.7 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 0.75 % Show Material materials with Kupfer of 0.75 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 30 - 35 % Show Material materials with Nickel of 30 - 35 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 0.15 - 0.6 % Show Material materials with Titan of 0.15 - 0.6 % |
Technological properties
Property | ||
---|---|---|
Processing history | hot-finished, annealed |