Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Chrom | 19.5 - 23.5 % Show Material materials with Chrom of 19.5 - 23.5 % |
Eisen | 21 - 37.9 % Show Material materials with Eisen of 21 - 37.9 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 1.5 - 3 % Show Material materials with Kupfer of 1.5 - 3 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 2.5 - 3.5 % Show Material materials with Molybdän of 2.5 - 3.5 % |
Nickel | 38 - 46 % Show Material materials with Nickel of 38 - 46 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.6 - 1.2 % Show Material materials with Titan of 0.6 - 1.2 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-finished, annealed |