Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 121 - 240 [-] Show Material materials with Härte, Brinell of 121 - 240 [-] | |
Härte, Rockwell B | 23.0 °C | 69 - 103 [-] Show Material materials with Härte, Rockwell B of 69 - 103 [-] | |
Härte, Rockwell C | 23.0 °C | 22 - 28 [-] Show Material materials with Härte, Rockwell C of 22 - 28 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Zugfestigkeit | 23.0 °C | 450 - 850 MPa Show Material materials with Zugfestigkeit of 450 - 850 MPa |