Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 45 - 55 % Show Material materials with Flächenreduzierung of 45 - 55 % | |
Härte, Rockwell B | 23.0 °C | 88 - 98 [-] Show Material materials with Härte, Rockwell B of 88 - 98 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Zugfestigkeit | 23.0 °C | 440 - 690 MPa Show Material materials with Zugfestigkeit of 440 - 690 MPa |