Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 20.0 °C | 20 % Show Material materials with Dehnung A5 of 20 % | |
Dehnung A5, transversal | 20.0 °C | 16 % Show Material materials with Dehnung A5, transversal of 16 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for High Carbon Steel |
Flächenreduzierung | 20.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % | |
Flächenreduzierung, transversal | 20.0 °C | 26 % Show Material materials with Flächenreduzierung, transversal of 26 % | |
Härte, Brinell | 20.0 °C | 152 [-] Show Material materials with Härte, Brinell of 152 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for High Carbon Steel |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze | 20.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa | |
Zugfestigkeit | 20.0 °C | 540 - 640 MPa Show Material materials with Zugfestigkeit of 540 - 640 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for High Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1289 - 1478 °C Show Material materials with Schmelzpunkt of 1289 - 1478 °C | Typical for High Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Eisen | 97.63 - 99.55 % Show Material materials with Eisen of 97.63 - 99.55 % |
Kohlenstoff | 0.6 % Show Material materials with Kohlenstoff of 0.6 % |
Mangan | 0.3 - 1.2 % Show Material materials with Mangan of 0.3 - 1.2 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | annealed, normalized or normalized and tempered |