Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 18 % Show Material materials with Dehnung A5 of 18 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Flächenreduzierung | 23.0 °C | 48 % Show Material materials with Flächenreduzierung of 48 % | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Schlagfestigkeit, Charpy gekerbt | 30.0 °C | 40 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 40 kJ/m² | |
Streckgrenze Rp 0,2 | 23.0 °C | 490 MPa Show Material materials with Streckgrenze Rp 0,2 of 490 MPa | |
Zugfestigkeit | 23.0 °C | 620 - 790 MPa Show Material materials with Zugfestigkeit of 620 - 790 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |