Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5, transversal | 23.0 °C | 13 - 16 % Show Material materials with Dehnung A5, transversal of 13 - 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Flächenreduzierung | 23.0 °C | 37 - 40 % Show Material materials with Flächenreduzierung of 37 - 40 % | |
Flächenreduzierung, transversal | 23.0 °C | 37 - 40 % Show Material materials with Flächenreduzierung, transversal of 37 - 40 % | |
Härte, Brinell | 23.0 °C | 229 [-] Show Material materials with Härte, Brinell of 229 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Streckgrenze | 23.0 °C | 570 - 600 MPa Show Material materials with Streckgrenze of 570 - 600 MPa | |
Zugfestigkeit | 23.0 °C | 780 - 930 MPa Show Material materials with Zugfestigkeit of 780 - 930 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |