Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 15 % Show Material materials with Dehnung A5 of 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 255 [-] Show Material materials with Härte, Brinell of 255 [-] | |
Härte, Rockwell C | 23.0 °C | 25 [-] Show Material materials with Härte, Rockwell C of 25 [-] | |
Härte, Vickers | 23.0 °C | 269 [-] Show Material materials with Härte, Vickers of 269 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 245 MPa Show Material materials with Streckgrenze Rp 0,2 of 245 MPa | |
Zugfestigkeit | 23.0 °C | 590 MPa Show Material materials with Zugfestigkeit of 590 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |