Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 5 - 20 % Show Material materials with Dehnung A5 of 5 - 20 % |
Härte, Vickers | 20.0 °C | 200 - 450 [-] Show Material materials with Härte, Vickers of 200 - 450 [-] |
Zugfestigkeit | 20.0 °C | 1030 - 1420 MPa Show Material materials with Zugfestigkeit of 1030 - 1420 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.5 % Show Material materials with Aluminium of 0.75 - 1.5 % |
Chrom | 16 - 18 % Show Material materials with Chrom of 16 - 18 % |
Eisen | 70.59 - 76.75 % Show Material materials with Eisen of 70.59 - 76.75 % |
Kohlenstoff | 0.09 % Show Material materials with Kohlenstoff of 0.09 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 6.5 - 7.75 % Show Material materials with Nickel of 6.5 - 7.75 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Processing history | as cold-rolled, or either as solution-treated or as annealed |