Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Vickers | 23.0 °C | 34 - 530 [-] Show Material materials with Härte, Vickers of 34 - 530 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 880 - 1320 MPa Show Material materials with Streckgrenze Rp 0,2 of 880 - 1320 MPa | |
Zugfestigkeit | 23.0 °C | 1140 - 1720 MPa Show Material materials with Zugfestigkeit of 1140 - 1720 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | as precipitation-hardened |