Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 8 - 10 % Show Material materials with Dehnung A5 of 8 - 10 % |
Flächenreduzierung | 20.0 °C | 60 % Show Material materials with Flächenreduzierung of 60 % |
Zugfestigkeit | 20.0 °C | 600 - 830 MPa Show Material materials with Zugfestigkeit of 600 - 830 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.35 % Show Material materials with Aluminium of 0.35 % |
Bor | 0.001 - 0.01 % Show Material materials with Bor of 0.001 - 0.01 % |
Chrom | 13.5 - 16 % Show Material materials with Chrom of 13.5 - 16 % |
Eisen | 49.13 - 59.5 % Show Material materials with Eisen of 49.13 - 59.5 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 1 - 1.5 % Show Material materials with Molybdän of 1 - 1.5 % |
Nickel | 24 - 27 % Show Material materials with Nickel of 24 - 27 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 1.9 % Show Material materials with Titan of 1.9 % |
Vanadium | 0.1 - 0.5 % Show Material materials with Vanadium of 0.1 - 0.5 % |