Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 20 - 25 % Show Material materials with Dehnung A5 of 20 - 25 % |
Flächenreduzierung | 20.0 °C | 65 % Show Material materials with Flächenreduzierung of 65 % |
Zugfestigkeit | 20.0 °C | 450 - 680 MPa Show Material materials with Zugfestigkeit of 450 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 17 - 19 % Show Material materials with Chrom of 17 - 19 % |
Eisen | 63.34 - 71.5 % Show Material materials with Eisen of 63.34 - 71.5 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 3 - 4 % Show Material materials with Kupfer of 3 - 4 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Nickel | 8.5 - 10.5 % Show Material materials with Nickel of 8.5 - 10.5 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |