Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 % Show Material materials with Dehnung A50 of 16 % | |
Dehnung A80 | 23.0 °C | 14 % Show Material materials with Dehnung A80 of 14 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Medium Carbon Steel |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 87 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 87 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 70 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 70 [-] | |
Härte, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Härte, Rockwell B of 80 [-] | |
Härte, Vickers | 23.0 °C | 170 [-] Show Material materials with Härte, Vickers of 170 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Medium Carbon Steel |
Schubmodule | 23.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Zugfestigkeit | 23.0 °C | 595 MPa Show Material materials with Zugfestigkeit of 595 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1380 - 1514 °C Show Material materials with Schmelzpunkt of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |