Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Steel |
Härte, Brinell | 23.0 °C | 152 - 201 [-] Show Material materials with Härte, Brinell of 152 - 201 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 - 494 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Wärmeleitfähigkeit | 23.0 °C | 23 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Technological properties
Property | ||
---|---|---|
Processing history | isothermally treated to ferrite-perlite structure and hardness range |