Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dehnung | 18.6 % Show Material materials with Dehnung of 18.6 % | Predicted Value, A80 | ||
18.7 % Show Material materials with Dehnung of 18.7 % | Predicted Value, Transverse | |||
19.5 % Show Material materials with Dehnung of 19.5 % | Predicted Value, A80 Transverse | |||
20 % Show Material materials with Dehnung of 20 % | ASTM A36 | Plate, Bar | A200 | |
21 % Show Material materials with Dehnung of 21 % | ASTM A36 | A50 | ||
23 % Show Material materials with Dehnung of 23 % | ASTM A36 | Plate, Bar | A50 | |
24.8 % Show Material materials with Dehnung of 24.8 % | Predicted Value | |||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||
Flächenreduzierung | 43.6 % Show Material materials with Flächenreduzierung of 43.6 % | Predicted Value, Transverse | ||
44.0 % Show Material materials with Flächenreduzierung of 44.0 % | Predicted Value | |||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||
Scherfestigkeit | 560.7 MPa Show Material materials with Scherfestigkeit of 560.7 MPa | Predicted Value | ||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||
Streckgrenze | 250 MPa Show Material materials with Streckgrenze of 250 MPa | ASTM A36 | Plate, Bar | |
266.7 MPa Show Material materials with Streckgrenze of 266.7 MPa | Predicted Value, RP05 | |||
278.4 MPa Show Material materials with Streckgrenze of 278.4 MPa | Predicted Value, RP1 | |||
303.5 MPa Show Material materials with Streckgrenze of 303.5 MPa | Predicted Value, Transverse | |||
316.1 MPa Show Material materials with Streckgrenze of 316.1 MPa | Predicted Value, RP1 Transverse | |||
324.8 MPa Show Material materials with Streckgrenze of 324.8 MPa | Predicted Value, RP02 | |||
441.6 MPa Show Material materials with Streckgrenze of 441.6 MPa | Predicted Value, RP002 | |||
496.5 MPa Show Material materials with Streckgrenze of 496.5 MPa | Predicted Value, RP02 Transverse | |||
Zugfestigkeit | 400 - 550 MPa Show Material materials with Zugfestigkeit of 400 - 550 MPa | ASTM A36 | Plate, Bar |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 341.1 °C Show Material materials with Max. Betriebstemperatur of 341.1 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 8 S/m Show Material materials with Elektrische Leitfähigkeit of 8 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Kohlenstoff | 0.26 % Show Material materials with Kohlenstoff of 0.26 % | ASTM A36 | Plate, Bar |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % | ASTM A36 | Plate, Bar |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | ASTM A36 | Plate, Bar |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % | ASTM A36 | Plate, Bar |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | ASTM A36 | Plate, Bar |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |