Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 260 [-] Show Material materials with Härte, Brinell of 260 [-] |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 1.4 - 1.8 % Show Material materials with Chrom of 1.4 - 1.8 % |
Kohlenstoff | 0.85 - 1 % Show Material materials with Kohlenstoff of 0.85 - 1 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 1.4 - 1.7 % Show Material materials with Mangan of 1.4 - 1.7 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Sauerstoff | 1.5E-3 % Show Material materials with Sauerstoff of 1.5E-3 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 - 0.8 % Show Material materials with Silizium of 0.5 - 0.8 % |
Titan | 5E-3 % Show Material materials with Titan of 5E-3 % |