Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 15.0 % Show Material materials with Dehnung of 15.0 % | Predicted Value, A200 |
15.4 % Show Material materials with Dehnung of 15.4 % | Predicted Value, A80 | |
18.3 % Show Material materials with Dehnung of 18.3 % | Predicted Value, Transverse | |
20.2 % Show Material materials with Dehnung of 20.2 % | Predicted Value, A80 Transverse | |
20.6 % Show Material materials with Dehnung of 20.6 % | Predicted Value, A5 | |
21 % Show Material materials with Dehnung of 21 % | Predicted Value, A50 | |
21.6 % Show Material materials with Dehnung of 21.6 % | Predicted Value | |
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Flächenreduzierung | 42.1 % Show Material materials with Flächenreduzierung of 42.1 % | Predicted Value |
43.0 % Show Material materials with Flächenreduzierung of 43.0 % | Predicted Value, Transverse | |
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Scherfestigkeit | 511.2 MPa Show Material materials with Scherfestigkeit of 511.2 MPa | Predicted Value |
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 315.4 °C Show Material materials with Max. Betriebstemperatur of 315.4 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 7 S/m Show Material materials with Elektrische Leitfähigkeit of 7 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Kohlenstoff | 0.23 % Show Material materials with Kohlenstoff of 0.23 % | ASTM A573 |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % | ASTM A573 |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | ASTM A573 |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | ASTM A573 |
Silizium | 0.1 - 0.35 % Show Material materials with Silizium of 0.1 - 0.35 % | ASTM A573 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |