Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dehnung | 17.5 % Show Material materials with Dehnung of 17.5 % | Predicted Value, A80 | ||
18 % Show Material materials with Dehnung of 18 % | ASTM A573 | Plate | A200 | |
18.1 % Show Material materials with Dehnung of 18.1 % | Predicted Value, Transverse | |||
19.3 % Show Material materials with Dehnung of 19.3 % | Predicted Value, A80 Transverse | |||
21 % Show Material materials with Dehnung of 21 % | ASTM A573 | Plate | A50 | |
23.1 % Show Material materials with Dehnung of 23.1 % | Predicted Value | |||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||
Flächenreduzierung | 43.6 % Show Material materials with Flächenreduzierung of 43.6 % | Predicted Value, Transverse | ||
43.8 % Show Material materials with Flächenreduzierung of 43.8 % | Predicted Value | |||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||
Scherfestigkeit | 534.7 MPa Show Material materials with Scherfestigkeit of 534.7 MPa | Predicted Value | ||
Schubmodule | 79.4 GPa Show Material materials with Schubmodule of 79.4 GPa | Predicted Value | ||
Streckgrenze | 265.5 MPa Show Material materials with Streckgrenze of 265.5 MPa | Predicted Value, RP1 | ||
288.6 MPa Show Material materials with Streckgrenze of 288.6 MPa | Predicted Value, RP05 | |||
290 MPa Show Material materials with Streckgrenze of 290 MPa | ASTM A573 | Plate | ||
315.9 MPa Show Material materials with Streckgrenze of 315.9 MPa | Predicted Value, RP1 Transverse | |||
329 MPa Show Material materials with Streckgrenze of 329 MPa | Predicted Value, Transverse | |||
372.1 MPa Show Material materials with Streckgrenze of 372.1 MPa | Predicted Value, RP02 | |||
411.9 MPa Show Material materials with Streckgrenze of 411.9 MPa | Predicted Value, RP002 | |||
484.2 MPa Show Material materials with Streckgrenze of 484.2 MPa | Predicted Value, RP02 Transverse | |||
Zugfestigkeit | 485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa | ASTM A573 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 12.1 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 12.1 1/K | Predicted Value |
Spezifische Wärmekapazität | 459.7 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 459.7 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 38.44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 38.44 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % | ASTM A573 | Plate |
Mangan | 0.85 - 1.2 % Show Material materials with Mangan of 0.85 - 1.2 % | ASTM A573 | Plate |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | ASTM A573 | Plate |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | ASTM A573 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | ASTM A573 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |