Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 23.0 °C | 40 - 45 % Show Material materials with Flächenreduzierung of 40 - 45 % |
Zugfestigkeit | 23.0 °C | 1450 - 2030 MPa Show Material materials with Zugfestigkeit of 1450 - 2030 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.35 - 0.6 % Show Material materials with Chrom of 0.35 - 0.6 % |
Kohlenstoff | 0.6 - 0.7 % Show Material materials with Kohlenstoff of 0.6 - 0.7 % |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.3 % Show Material materials with Silizium of 0.15 - 0.3 % |
Vanadium | 0.1 - 0.25 % Show Material materials with Vanadium of 0.1 - 0.25 % |