Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 23.0 °C | 30 - 40 % Show Material materials with Flächenreduzierung of 30 - 40 % |
Zugfestigkeit | 23.0 °C | 1690 - 2370 MPa Show Material materials with Zugfestigkeit of 1690 - 2370 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 - 0.8 % Show Material materials with Chrom of 0.5 - 0.8 % |
Kohlenstoff | 0.55 - 0.68 % Show Material materials with Kohlenstoff of 0.55 - 0.68 % |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 1.2 - 1.65 % Show Material materials with Silizium of 1.2 - 1.65 % |
Vanadium | 0.08 - 0.25 % Show Material materials with Vanadium of 0.08 - 0.25 % |