Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 22 % Show Material materials with Dehnung A50 of 22 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Kerbschlagenergie | 23.0 °C | 18 J Show Material materials with Kerbschlagenergie of 18 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 450 MPa Show Material materials with Streckgrenze of 450 MPa | |
Zugfestigkeit | 23.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.06 % Show Material materials with Aluminium of 0.06 % |
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % |
Mangan | 1.15 - 1.5 % Show Material materials with Mangan of 1.15 - 1.5 % |
Molybdän | 0.05 % Show Material materials with Molybdän of 0.05 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.1 - 0.35 % Show Material materials with Silizium of 0.1 - 0.35 % |
Vanadium | 0.12 % Show Material materials with Vanadium of 0.12 % |