Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Kerbschlagenergie | 23.0 °C | 18 J Show Material materials with Kerbschlagenergie of 18 J | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 335 - 481 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 % Show Material materials with Chrom of 0.5 % |
Kobalt | 0.5 % Show Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 0.6 % Show Material materials with Mangan of 0.6 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 35 - 37 % Show Material materials with Nickel of 35 - 37 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.35 % Show Material materials with Silizium of 0.35 % |