Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 16.5 - 30 % Show Material materials with Dehnung A50 of 16.5 - 30 % |
Kerbschlagenergie | 23.0 °C | 18 J Show Material materials with Kerbschlagenergie of 18 J |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa |
Zugfestigkeit | 23.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.04 - 0.3 % Show Material materials with Aluminium of 0.04 - 0.3 % |
Chrom | 0.44 - 1.01 % Show Material materials with Chrom of 0.44 - 1.01 % |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Kupfer | 0.4 - 0.75 % Show Material materials with Kupfer of 0.4 - 0.75 % |
Mangan | 0.5 - 1.05 % Show Material materials with Mangan of 0.5 - 1.05 % |
Nickel | 0.47 - 0.98 % Show Material materials with Nickel of 0.47 - 0.98 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.08 - 0.37 % Show Material materials with Silizium of 0.08 - 0.37 % |