Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Härte, Brinell | 23.0 °C | 163 [-] Show Material materials with Härte, Brinell of 163 [-] |
Härte, Rockwell B | 23.0 °C | 85 [-] Show Material materials with Härte, Rockwell B of 85 [-] |
Streckgrenze | 23.0 °C | 205 MPa Show Material materials with Streckgrenze of 205 MPa |
Zugfestigkeit | 23.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.3 % Show Material materials with Kohlenstoff of 0.3 % |
Mangan | 0.4 - 1.06 % Show Material materials with Mangan of 0.4 - 1.06 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |