Mechanisch
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.75 - 1.25 % Show Material materials with Kupfer of 0.75 - 1.25 % |
Mangan | 0.4 - 1.06 % Show Material materials with Mangan of 0.4 - 1.06 % |
Nickel | 1.6 - 2.24 % Show Material materials with Nickel of 1.6 - 2.24 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |